Showing the single result
Measuring Principle: Cantilever bending method
Test Parameter: Bending length / Stiffness
Specimen Width: Typically 25 mm (as per standards)
Specimen Length: Adjustable
Measurement Range: Suitable for low to high stiffness materials
Scale Type: Direct reading scale / Graduated scale
Accuracy: High precision with repeatable results
Operation: Manual / Semi-automatic (model dependent)
Construction: Rigid metal body with corrosion-resistant finish
Clamping System: Precision specimen holder for accurate positioning
Standards Compliance:
ISO 2493
TAPPI T489
BS 3748
Paper & Paperboard testing
Packaging material evaluation
Carton & corrugated box testing
Printing & publishing industry
Quality control & R&D laboratories
Username or email address *Required
Password *Required
Log in
Lost your password? Remember me
No account yet?